Stretch film is made to do exactly what the name implies, stretch. By stretching a stretch film to the maximum stretch rate, companies save money on film costs and reduce product loss. Hand and machine stretch film offer different stretch rates. Resin formulas and brand varieties offer different stretch rates. With the simple steps below, companies can find out the amount of stretch being reached by hand or machine applications.

This is a great resource to use to be sure a machine is reaching the maximum stretch rate. It is also a great way to find out if workers are attaining the proper amount of stretch when applying hand film. Use this as a method of auditing and decreasing film usage.

Tools and Materials Needed

We recommend using a pallet of goods that are commonly wrapped. Remember that uniform pallet loads such as boxesSupplies Needed will often obtain a higher stretch rate than loads with sharp edges or corners.

Ruler - Used for Drawing a straight line

Marker - Preferably a permanent marker

Tape Measure - To measure lines

Calculator - For simple math

Pen and Paper - To write down measurements

Step One

Tie the stretch film to the corner of the pallet and make one or two full revolutions around the pallet.

Stretch Film Tied To Pallet

 

Step Two

After the last corner is reached to complete two full revolutions, loosely pull 5-6 ft. from the stretch film roll and hold up to the pallet.

Loose Stretch Film

Step Three

Hold the loose stretch film up to the boxes and make 3-5 lines ten inches long on different sides of the film. The lines should be spaced apart a few inches across the length of the extra film pulled out in step two. Making a ten-inch line makes doing the math much easier once the test is complete. Multiple lines should be marked on the film to obtain an average rate during one revolution of pallet wrapping.

Making lines on stretch film

How it should look when completed

Finished lines on the film

Step Four

Wrap the pallet as normal after 3-5 ten inch lines are marked on it. This can be done by hand or with a machine. After the pallet is wrapped the lines should be stretched out longer than the original 10 inches.

Wrapped Pallet

Step Five

Use a tape measure to measure the stretched lines and write each line length down.

Measuring lines of wrapped pallet

Step Six

After all of the stretched lines are measured and wrote down, get the average length of the lines by adding all lengths together and dividing by the number of lines. If the average of all of the lines is 20, a 100% stretch rate is being reached. If the average of the lines is 30 inches, a 200% stretch rate is being reached.

This is by no means a scientific method for testing the stretch rate of pallet wrap. The proper tools and equipment needed for scientific testing can be expensive. This is merely an easy way to audit film stretch rates. This will help forecast film usage as well as signal possible adjustments that may need to be made when wrapping pallets in the warehouse. Call us at 1-800-441-5090 with questions about stretch film, stretch wrap machines or anything else related to unitized load packaging.